ACID RESITANT BRICK
ACID RESITANT BRICK FOR CHIMNEY
Chemical Composition and Physical Properties:
Items Index SiO2 70 ± 5% Al2O3 20% min Fe2O3 7% max Acid Resistance 98% min Soaked in 5 ~ 6% Sulfuric Acid 30 days and strength reduction shall be less than 5% Bulk Density 1.9 ± 0.05 g/cm3 Compressive Strength 20 Mpa min Refractoriness 1300°C Water Absorption 17% max